In Topic: How To Turn Cobalt Blues Into Something Much More Subtle?

23 March 2014 - 02:44 PM

Hey Oly - found this on pinterest.  Not sure who was the originator but does this help?  You will have to translate the ingredients though.

http://media-cache-e...1752834af90.jpg


In Topic: Native Clay Glaze

06 March 2014 - 08:06 PM

This is my native clay - a red terra cotta.  Recipe - terra cotta 80; Frit 3134 20.

You can see the little tea dust crystals.

 


In Topic: Clay And Shale Resources Of Ontario

23 February 2014 - 01:24 PM

OK - let's see if this works - trying to add the photo of the glaze


In Topic: Clay And Shale Resources Of Ontario

23 February 2014 - 01:20 PM

Hey Tyler - I use this doc a lot.  I get run off clay from around Terra Cotta and make a nice brown glaze with the addition of 20% 3134 frit.


In Topic: Mastering Cone 6 Glazes - Priced Way Out

06 January 2014 - 09:22 PM

Not sure why this didn't post - Tuckers Pottery in Ontario may still have copies  $ 40 Cdn.