My big skutt gave up last night, after 15 hours only made it to 2000 degrees, time to rewire ugh!
Jul 02 2017 08:41 AM
  • Denice's Photo
    Denice
    I would even say elementary Watson.
    Jul 02 2017 10:16 PM
  • S. Dean's Photo
    S. Dean
    Coiled again
    Jul 03 2017 10:47 AM
  • Min's Photo
    Min
    Don't get wound up over it.
    Jul 03 2017 04:21 PM
Photo

DeniceTJR

TJR I thought I would let you know they have moved the warning south of us. I'm not really worried about myself just everyone else. I have a basement to hide in some people have no where to go. A large tornado the other night north of Wichita was mostly in no mans land. But it took out three farms and killed 1500 cattle. All 3 families lost their lively hood, no one insures cattle. De...
May 30 2013 12:03 PM
Photo

TJRDenice

Denice;
I'll be thinking about you during this tornado season.Good luck and take care.
Tom.
May 30 2013 10:03 AM
Photo

DenicePugaboo

Hi I have enjoyed your pug sculptures, I did portraiture sculpture for years. I wanted to tell you about SmartFlix.com you can rent educational DVD's they have quite a few pottery dvd's. I have never used them but I thought you should know about them. Denice
Mar 21 2013 09:14 AM

Denice

Hello! No I don't have a studio yet. I'm in the middle of selling some industrial equipment and as soon as it sells, God willing, I will be buying a wheel and kiln : ). I had a kiln that I sold back in 94. I had gotten it used from a friend's mom. I use to do the ceramic mold thing. It was fun.
Feb 26 2013 11:07 AM
Photo

DeniceTJR

TJR That particular fountain is Cone 1 Majolica and low fire red terracotta that is fired to it's max temp. to make it vitrified and hold up to freezing weather. The spills and moldings are Cone 6, I worked on the low fire glaze and clay combination development for 6 months. I wanted it vitrified and not crazing which is what Majolica does. I have done 3-3' and 2-6' murals also w...
Jan 10 2013 02:01 PM
Photo

TJRDenice

Denice; Had to look at your work since you mentioned double firing dowm - or something technical like that. Like the yellow.
Tom.
Jan 10 2013 10:18 AM
Photo

SShirleyDenice

Denice,
Thanks for writing. I accidentally deleted the message before I finished reading all of it, but I appreciate your kind support. It boggles the mind that Mia is the moderator. She seems a little overly critical, and I am overly sensitive, so that is a bad combination. I did get a lot out of the rest of the posts though. I hope you have a great Christmas holiday!
Dec 23 2012 11:49 AM
Photo

TJRDenice

Denice;
Wow, you are really old! I am hitting the big 6-0 this July 13. Have a very Happy Birthday.
Tom Roberts[TJR]
Oct 18 2012 04:44 PM
Photo

Denicepkbrier

Hi PK what city are you near. I am from Wichita and there's another potter on this forum from Pittsburg. If you have more questions about setting up your studio you can e-mail me directly. I work in Cone 6 electric and could help you get started with it. Denice
Feb 23 2012 09:30 AM