Glaze Warping Pots

11 November 2013 - 03:07 PM

I have glazed a few pots with a glaze made of 50/50 ash and ball clay. The clay is warping round bowls into tacos (both stoneware and porcelain, made by me and by someone else). I guess this is a fit issue, right? Is there something I should consider adding to rectify the issue? I should add that I know very little about glaze chemistry. 

Warren Mackenzie Platter Decorating Technique

30 September 2013 - 11:32 AM

There's a specific thing that Warren sometimes does on some of his platters, these lines that are thick on the ends and thin in the middle, and I wonder if people think that this is just done with a brush, or it's poured, or what. I provide links to 3 examples below.