Hello, I would like to find recipes and methods for developing my own arts and crafts style MATTE glazes. They seem to be hard to find on the general web. Can some one supply me with a basic starter recipe, cone 6, and a path or direction I can follow in developing my own glazes...principles, tips, website, book, etc.

 

thank you very much, paul

Share this post


Link to post
Share on other sites
bciskepottery    925

These are the books I use/recommend most often:

 

Mastering Cone 6 Glazes by John Hesselberth and Ron Roy, The Complete Guide to High-Fire Glazes by John Britt, and Cushing's Handbook by Val Cushing (availabe from the author).

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

If you go to my gallery on this site, I posted a picture and a recipe of such a glaze. I have found the matte glazes in Michael Bailey's ^6 recipes to be a good starting point.

here is the link to my gallery picture with comment.

The comment is the recipe.

http://ceramicartsda...ewimage&img=778

 

Marcia

Share this post


Link to post
Share on other sites

These are the books I use/recommend most often:

 

Mastering Cone 6 Glazes by John Hesselberth and Ron Roy, The Complete Guide to High-Fire Glazes by John Britt, and Cushing's Handbook by Val Cushing (availabe from the author).

 

 

 

Thank you...Mastering cone 6 glazes is at the top of my wish list on Amazon...just need to take a deep breath and hit Buy.

Share this post


Link to post
Share on other sites

If you go to my gallery on this site, I posted a picture and a recipe of such a glaze. I have found the matte glazes in Michael Bailey's ^6 recipes to be a good starting point.

here is the link to my gallery picture with comment.

The comment is the recipe.

http://ceramicartsda...ewimage&img=778

 

Marcia

 

 

 

Thank you Marcia for sharing your recipe, I really like it...beautiful plate. This is in the direction where I want to go. Thanx again.

 

paul

Share this post


Link to post
Share on other sites
Pam S    6

Hit the oreder button! That book is worth every penny!

 

@Marcia, thanks for the recipe! I've been looking for a lighter green and that is it!

 

 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×