Ann E. V.

Sodium Silicate

Recommended Posts

Ann E. V.    0

is sodium silicate supposed to be dry crystals or liquid when added to formulas?? mine came in a pint container with small amount of liquid at the top and a rock hard crystalline pack underneath. No amount of stirring, scraping or shaking will change this consistancy. When a recipe calls for sodium silicate do I pour off and measure the liquid at the top or chip out the solid stuff at the bottom??

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

I think it may have passed its shelf life. When my sodium silicate looks like it is separating, I use a small jiffy mixer to stir it up. If you can't rester it, I think it has passed the shelf life.

Marcia

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×