oldlady Posted October 2, 2016 Report Share Posted October 2, 2016 you mention having "some school buff" clay. can you ask the person who gave you the clay since they would know the most about it. if not, you might contact a local paint your own pottery location. ask questions. you will probably find that bisque is fired to cone 06, yes, the same cone as the final glaze firing. i cannot help beyond this. i have not done any work in earthenware in a half century. you probably also have a local library where there are many books telling all about this subject. working with clay is such a vast field that you might benefit from an overview such as you would find in any good, textbook type, reference book. Link to comment Share on other sites More sharing options...