I consistently fire about a half cone cooler in the top and bottom of my Olympic 2327HE single zone kiln,   Watching loading and shelf spacing helps but doesn’t eliminate the situation.

I was wondering if it’s possible to simply add two new T/Cs and split the relay outputs to convert the Bartlett Controller to three zone control.  As far as I can determine the actual controller board is standard and determines zone control based on how T/Cs are connected.  

Any help would be appreciated.     Yes, I know this voids the warrenties.

Link to comment
Share on other sites

Yes, you can add TC's and wire it appropriately. I assume the controller is a Bartlett V6-CF? Refer to the manual for how to program for the number of zones you have. It won't automatically recognize the TC's, you have to program it. I think Bartlett has wiring diagrams on their site. While you're at it, put in protection tubes for the TCs.

Link to comment
Share on other sites

I consistently fire about a half cone cooler in the top and bottom of my Olympic 2327HE single zone kiln,   Watching loading and shelf spacing helps but doesn’t eliminate the situation.

I was wondering if it’s possible to simply add two new T/Cs and split the relay outputs to convert the Bartlett Controller to three zone control.  As far as I can determine the actual controller board is standard and determines zone control based on how T/Cs are connected.  

Any help would be appreciated.     Yes, I know this voids the warrenties.

Hi Marvin,

You can add T/C's and rerout the wires to the relays from the board, you also need some type K extension wire for the new TC's  You will need the code to get in deep enough to reprogram for zone control, unless that has allready been done and single zone was chosen for your kiln.  Look at the posts on metal spitting from thermocouple, I am not in agreement about using a mullite protection tube and the offset you have to put in the controller.  I don't have any offset on mine, and get great results. My thermocouple is in a metal Omegaclad tube.

David

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.