Hello all...

This morning I woke up and I went to check how my pieces were doing. I made two batches, one copper oxide and one maganese oxide. 

The copper oxide efflorescence has started, but it looks very strange.... Is this normal or does anyone have any ideas?? It looks a lot different to the other pieces.

 

Formula: 

90g silica

5g soda

5g lime

2.2g copper oxide 

 

7g ball clay 

30ml water 

 