sparklingmango Posted April 17, 2015 Report Share Posted April 17, 2015 Yo! Oxides are cool....I thought it would be cool to start a thread on oxides. (Sorry if there is already one!)I made a faience mixture today with 1.2% manganese into the mix, is this going to be a pinky, purpely thing??Any oxide recommendations..... Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted April 17, 2015 Report Share Posted April 17, 2015 Likely brown or black. Link to comment Share on other sites More sharing options...
TJR Posted April 17, 2015 Report Share Posted April 17, 2015 If you combine chrome with tin you will get pink over certain glazes. Can't tell you the percentages. 1% chrome to 2% tin? Maybe. Copper carb and tin-same ratio. TJR. Link to comment Share on other sites More sharing options...