CactusPots Posted July 2, 2020 Report Share Posted July 2, 2020 An alternative to clay cookies is to cut soft brick into cookies. You really need a bandsaw to do this properly, so that will probably kill this suggestion for a lot of people. Pretty quick way to set up a box full of exact same size thickness goodness that can be used over and over. At least until a glaze drip claims it's life. Even then the soft brick is easier to grind than clay. Link to comment Share on other sites More sharing options...