I tried the Paladium recently at cone 5; gave a mirror like look I personally found I did not care for.



#42 JLowes

JLowes

    Clay Doodler

  • Members
  • PipPipPip
  • 267 posts
  • LocationAtlanta Georgia area

Posted 25 September 2015 - 12:08 PM

If cone 05 wasn't completely collapsed, then you did not get the firing temp required for Saturation gold. Does your kiln have a sitter for shut off? If it does you may have an 05, not 6, in the sitter shutting you off way early. Make sure you have a small cone 6 in the sitter and try it again.