Argosworks Posted February 25, 2015 Report Share Posted February 25, 2015 Our studio has been using Glazemixer in the past and it is obvious to us that we cannot get our glaze from Glazemixer any more. We are now using another vender to mix our dry glazes. The problem we are having is that we do not have access to some of our favorite glazes - Green Pooling Blue and Mother of Pearl. Do anyone know how we can get these glazes and if we can get the recipe for them. Does anyone use the Hobart Cowles Fluid Blue-Green Glaze in the Cone 5-6 Glazes (pg 118)? If you have used it could you post a photo of it and give the type of clay. We would like to know the HC B-G is like Green Pooling Blue? Thanks for any help Ginny J Clay Artists at the Vineyard San Diego, CA Link to comment Share on other sites More sharing options...
bciskepottery Posted March 1, 2015 Report Share Posted March 1, 2015 John Britt's new book, The Complete Guide to Mid-Range Glazes, has a blue/green on pages 112-113 called Arrowmont Blue Green. It is a titanium green and uses titanium green and cobalt carbonate to achieve the colors. Link to comment Share on other sites More sharing options...
Argosworks Posted March 6, 2015 Author Report Share Posted March 6, 2015 Thank you, I have used Green Pooling Blue with Gloss White and have some interesting results. The Green Pooling Blue is a runny glaze. Here an example of the glazes together. Link to comment Share on other sites More sharing options...
Tileworks Posted October 15, 2016 Report Share Posted October 15, 2016 So this is a very old thread, but I was vanity Googling around and found it. Green Pooling Blue and Mother of Pearl were created by me. Both were developed for my tile studio over a long period of testing. I can't tell you how tickled I am to find people who appreciate the work I put into developing them. Glazemixer was a pretty cool service and I'm sad that it's gone. Link to comment Share on other sites More sharing options...
Mark C. Posted October 16, 2016 Report Share Posted October 16, 2016 So this is a very old thread, but I was vanity Googling around and found it. Green Pooling Blue and Mother of Pearl were created by me. Both were developed for my tile studio over a long period of testing. I can't tell you how tickled I am to find people who appreciate the work I put into developing them. Glazemixer was a pretty cool service and I'm sad that it's gone. The original poster is asking for the recipe-Do you want to post it here? I'm a cone 10 guy so this would be for the midrange folks Link to comment Share on other sites More sharing options...
Tileworks Posted October 18, 2016 Report Share Posted October 18, 2016 Hi Mark. Sorry, I'm not the sole owner of the recipe and I don't have permission to post it. If we had something else like glazemixer I think we could do what we were doing before, just selling it premixed without handing out the formula. I'm just happy to see that someone enjoyed the fruits of our labor :-) Link to comment Share on other sites More sharing options...
Min Posted October 30, 2016 Report Share Posted October 30, 2016 Don't know if the original poster is still checking this thread or not but I think the glaze below may work as a substitute. I would increase the cobalt from 0.5 to up to about 1.25 and go from there with testing. Original glaze (pictured on Electric Cone 6 site) Possible recipe swap on the left: http://glazy.org/recipes/3897 Link to comment Share on other sites More sharing options...
Argosworks Posted November 19, 2016 Author Report Share Posted November 19, 2016 To Tileworks you Post: Sorry, I'm not the sole owner of the recipe and I don't have permission to post it. If we had something else like glazemixer I think we could do what we were doing before, just selling it premixed without handing out the formula. I'm just happy to see that someone enjoyed the fruits of our labor :-) This is Argosworks who wanted these glazes. I am still looking for the two glazes. I talked to Ryan from Glazemixer and asked if he would send a note to the owner of the glazes to contact me so that I could buy the premixed glaze. Ryan refused to contact the owner of the glaze for me. Are you the owner of the glaze? Can I get a small sample of the premixed glaze and I would pay for the sample and shipping. Link to comment Share on other sites More sharing options...
Tileworks Posted February 21, 2017 Report Share Posted February 21, 2017 Sorry it took me forever to see your post & respond. Yes, my partner and I developed the glaze for our tile studio. I'm not actually in the business of mixing & selling glazes. My grammar in my last post wasn't so great. I was trying to say that if there was a new Glazemixer I would be willing to share the glaze through there. My deal with my partner doesn't allow me to share the actual formula freely. Ryan seems like a good guy. I'm sorry his business didn't work out. I miss Glazemixer! The glaze from Glazy posted above does look worth trying. I didn't see anything there that looks like the mother of pearl glaze there. Did you see any candidates? Link to comment Share on other sites More sharing options...
Tileworks Posted February 21, 2017 Report Share Posted February 21, 2017 For a pearl glaze maybe try this one- Behrens Pearl White https://glazy.org/recipes/2626 Link to comment Share on other sites More sharing options...
texasadam Posted May 18, 2017 Report Share Posted May 18, 2017 I thought the glazes posted on Glazemixer were posted by users and they included the recipe. They would mix any glaze that was posted in the forums. Maybe i'm wrong. I wish they had just left the forums up so that users like myself could still get the recipes. I bought a glaze from Glazemixer called "wood ash traditional shino" and wish I had the recipe - I just used the last of it! Link to comment Share on other sites More sharing options...
Argosworks Posted May 20, 2017 Author Report Share Posted May 20, 2017 Tileworks When I talked to Ryan of Glazemixer and asked about the Green Pooling Blue, he did not want to let me to have the contact. I understand not wanting to give me the email of the person who owns Green Pooling Blue, so I asked that he would send my email have the owner so I could contact the own. Could I use another vendor to mix the glaze and I would pay in the same way that Glazemixer took 10% fee for using the glaze recipe? We have a relationship with a vendor who mixes the glazes for us. We would not have the recipe, but only the glaze mixer would have the recipe. I use Green Pooling Blue on top of a white glaze. The result are beautiful!!! Thanks for thinking about this. Link to comment Share on other sites More sharing options...
Argosworks Posted May 23, 2017 Author Report Share Posted May 23, 2017 DEAR TILEWORK, WE WOULD LIKE TO PURCHASE THE TWO GLAZES PRE-MIXED ( GREEN POOLING BLUR, MOTHER OF PEARL) FROM YOU. HOW MUCH WOULD IT COST? WE ARE IN SAN DIEGO, CA. THANK YOU. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted May 24, 2017 Report Share Posted May 24, 2017 Dear Argoworks I think it would be better if you private emailed or directly contacted Tileworks. This forum is not set up for business transactions Marcia Talk Business (Don't Do Business) Started by Guest_Sherman_* , Aug 15 2010 05:47 PM This topic is locked This topic is locked No replies to this topic #1 Talk Business (Don't Do Business): post #1 Guest_Sherman_* Guests Posted 15 August 2010 - 05:47 PM This is just a friendly reminder that this forum is for discussing all things relating to the business of ceramic art. The one thing it is not intended for is the actual conducting of business. For that, we have the very convenient, and more appropriate, classified ad page: http://ceramicartsda...ly/classifieds/ Thanks for your understanding and cooperation. Sherman and the admin/mod team Link to comment Share on other sites More sharing options...