I work with commercially prepared earthenware clay and sometimes slipcast with a different brand. The broken pieces have ended up in the same bucket. Will my reclaimed clay be ruined?

 

 

***Warning, I am still doing experiments and am only a beginner at trying this

 

I have recently done this on purpose, similar happenstance but my clay is a pressing clay, my slip a different brand that we have not been able to get so we were running low.

 

I have no idea what I was doing so I googled making slip and am in the trial and error phase of seeing if I can combine lots of scarp pressing clay (pug mill is out of service and I have rebuilding it, plus it scares me to death)

 

I started with this link here

 

http://www.nmclay.com/Customer_service/Slipmaking.htm

 

I narrowed the list down a bit as I knew my pressing clay had some of the ingredients and we have a super osmosis water filter dohicky at our studio

 

so far the only thing I have added is a bit of soda ash (using Arm & Hammer washing soda as it has no additives and is Sodium Carbonate - soda ash)

 

Wish I would have kept better track of the amounts for future reference as I sort of just guessed.

 

I did a test casting of pure recycled and it came out of mold fine, I've since added a about 4 gallons of it to my existing slip and it has cast fine too.

 

My first test piece is in kiln as I write this as I'm hoping I have no problems with glaze fit as I added no talc as I figured my pressing clay and the existing slip had it already.

 

So far so good.

 

here is another resource I used as it has a bit more info on adjusting. I'm a googler, when I need to figure out something I just google like crazy.

 

http://www.lagunaclay.com/support/art-of-slipmaking.php

 

 

 

 

 

Share this post


Link to post
Share on other sites

Thanks for the info. I hope your experiment is a success.

 

 

 

 

I work with commercially prepared earthenware clay and sometimes slipcast with a different brand. The broken pieces have ended up in the same bucket. Will my reclaimed clay be ruined?

 

 

***Warning, I am still doing experiments and am only a beginner at trying this

 

I have recently done this on purpose, similar happenstance but my clay is a pressing clay, my slip a different brand that we have not been able to get so we were running low.

 

I have no idea what I was doing so I googled making slip and am in the trial and error phase of seeing if I can combine lots of scarp pressing clay (pug mill is out of service and I have rebuilding it, plus it scares me to death)

 

I started with this link here

 

http://www.nmclay.co.../Slipmaking.htm

 

I narrowed the list down a bit as I knew my pressing clay had some of the ingredients and we have a super osmosis water filter dohicky at our studio

 

so far the only thing I have added is a bit of soda ash (using Arm & Hammer washing soda as it has no additives and is Sodium Carbonate - soda ash)

 

Wish I would have kept better track of the amounts for future reference as I sort of just guessed.

 

I did a test casting of pure recycled and it came out of mold fine, I've since added a about 4 gallons of it to my existing slip and it has cast fine too.

 

My first test piece is in kiln as I write this as I'm hoping I have no problems with glaze fit as I added no talc as I figured my pressing clay and the existing slip had it already.

 

So far so good.

 

here is another resource I used as it has a bit more info on adjusting. I'm a googler, when I need to figure out something I just google like crazy.

 

http://www.lagunacla...-slipmaking.php

 

 

 

 

 

 

Share this post


Link to post
Share on other sites

That was a long story but I think you will be fine. Not sure how much of a mix you have though.

 

I've recently just ordered some sodium Silicate liquid for another deflocculate besides the soda ash just in case I get too thick as I've started on the second 5 gallon bucket.

 

Figure if I fail and it does not cast well I'll just make a bunch of paper clay with it.

Share this post


Link to post
Share on other sites

I work with commercially prepared earthenware clay and sometimes slipcast with a different brand. The broken pieces have ended up in the same bucket. Will my reclaimed clay be ruined?

 

 

I teach where there is lots of different clays discarded by the wheel throwers. I wedge and recycle and sculpt with all the clays. I only low fire and have had no problems. I also love slipcast clay for repairs which I apply to all clays and there's never been a rejection or crack. Try some small tests and see if you like the results.

Share this post


Link to post
Share on other sites

the thing that one must be apprehensive of when mixing two clay bodies is that there are different kinds of kaolins and fluxes in each clay body. a small amount of different clay will not make a difference but over a long time it will also if you mix 1/2 and 1/2 you may have molecular issues or maybe lowering the melting point or worse.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.