D.M.Ernst Posted February 6, 2015 Report Share Posted February 6, 2015 My very badly warped and glaze-covered shelves functioned as garden sculpture for about six years. Imagine four 20" half shelves "glued" to their posts creating one piece. Quite funky actually. I broke them apart and currently three of them are serving as the "shelves" for the waterfall that flows into our backyard pond. They've worked nicely for two years. No pictures because they're under 15" of snow right now. Link to comment Share on other sites More sharing options...
Mark C. Posted February 6, 2015 Report Share Posted February 6, 2015 If you buy the diamond wheel be carefull as it will grind into those mulite shelves like hot knife thru butter. Mark Link to comment Share on other sites More sharing options...