High Bridge Pottery Posted January 22, 2015 Report Share Posted January 22, 2015 Does storing oxides in direct sunlight affect them in any way? Link to comment Share on other sites More sharing options...
TJR Posted January 22, 2015 Report Share Posted January 22, 2015 No. Just store them in a dry container with a tight fitting lid. Metal coffee cans are good, or those one gallon ice cream pails.[the plastic ones]. Any free container with a re-sealable lid will work. TJR. Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted January 22, 2015 Author Report Share Posted January 22, 2015 This is my new organised oxides, used to use most from the bag they came in. Something like this should be ok? Not really in direct sunlight for that long. Link to comment Share on other sites More sharing options...
bciskepottery Posted January 22, 2015 Report Share Posted January 22, 2015 I use similar plastic containers with lids. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.