Chris Campbell Posted January 6, 2015 Report Share Posted January 6, 2015 I have just posted some images of the results of my experiments with throwing colored clay on my blog. http://www.ccpottery.com/blogs--and-life-its-own/ I hope those of you who might be interested in taking thrown colors past the simple "mash together and throw marbled" will enjoy playing with my ideas and maybe even reporting back on your progress/discoveries. I know I likely will not get time back with this project until the fall so I wanted others to have a chance to take my work further. I used to think you needed great throwing skills to work with color patterns but it turns out you don't. I cannot wait to see what some good throwers can do with my basic ideas. Link to comment Share on other sites More sharing options...
Crusty Posted January 7, 2015 Report Share Posted January 7, 2015 Pretty color, i seen a guy wedge 3 different clays together one way then threw them the other way.. cool stuff.. what do you color the clay with? Link to comment Share on other sites More sharing options...
Chris Campbell Posted January 7, 2015 Author Report Share Posted January 7, 2015 Here is a link to all of the information on colored clay on my site .... http://ccpottery.com/murrinis.html Link to comment Share on other sites More sharing options...
Crusty Posted January 9, 2015 Report Share Posted January 9, 2015 neat. i like the mixer picture, we have a nice cake mixer that saves alot of time making slip lol... not a Hobart though, that thing will last forever... Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.