DirtRoads Posted December 26, 2014 Report Share Posted December 26, 2014 Getting new Advancers for my new L&L. In current set up I have those other types of shelves on the bottom row. Advancers on the other rows. Seems I remember getting advise to use the white shelves on bottom ..... is this accurate? Link to comment Share on other sites More sharing options...
Mark C. Posted December 26, 2014 Report Share Posted December 26, 2014 I'm not sure why you would not want all advancers as they save space. The other shelves would keep more thermo mass (warm) than advancers but why would you need it?Save space = money and fuel saved-I have all advancers in my two reduction kilns including the floor. Now those advancers will not like thermo shock if your kiln vent system draws in cold air but I cannot see this as much as a shock. Mark Link to comment Share on other sites More sharing options...