hello I work at a paint your own pottery store and the trouble we seem to be having with certain pieces is that the glaze seems to flake off work almost crack like an egg shell and we are unsure how to fix it or even why this happens any help or suggestions are very very welcome we fire to cone 05 and we used Duncan glazes

Link to comment
Share on other sites

We need a few more details . . .

Is the glaze flaking off the bisque ware or after being glazed fired?

Is this a problem with all glazes, or just a particular glaze?

Are the glazes newly mixed? Or one's that have been around for a while?

With a variety of forms or just one form?

And, if you could post a picture, that would truly help provide an answer.