I have a question that I hope someone will be able to answer. As a newbie in the world of "ceramic molds" I came across some cartoon characters ceramic molds such as Mickey Mouse, Donald Duck, and Pinnochio to name a few.  Although I'm not ready to learn how to use them yet, what is the best way to store them.  I should mentioned that the molds I have have two pieces.  I have read conflicting information that the molds should be stored upright with the pouring hold faced down to laying the ceramic mold flat (on the flat side of the mold) with the seam line (I'm assuming this is where each side of the mold meets) should be parallel and not stored this way. 

 

Thank you in advance.

Link to comment
Share on other sites

I read that you should store moulds "face to face".  That is with the pouring holes facing each other.  Something to do with the salts leaching outwards not inwards.  Also helps to keep the creatures and dust out.  At this time of year my studio has a coating of Silver Birch seeds.  In the spring it's spiders and pollen.  If they're stored on solid shelves in a single layer, they could be face down.

 

Whichever way up they are, they need to be banded together, not left in separate parts.

Link to comment
Share on other sites

  • 1 month later...
  • 3 months later...

I also have a mold storage question :)

 

Can i storage plaster molds that i rarely use outside in a shed? Im located in northern EU, so 4 seasons and temps between -4f to 85f.

Well, acutually i have used old molds that were kept years  in a moist basement, i dried them, and saw no difference in setting times.

But still... :huh:

Link to comment
Share on other sites

  • 2 months later...

speaking of molds I have a bunch under my house that I'm recycling(small truck full)

They are getting ground up with cement and other road fill at a recycle plant down the road.

These mold are from my collage days and are of unsual forms like donuts and dog poo and bread loafs ( it was art).

Mark

Link to comment
Share on other sites

  • 4 years later...

I have a question.

I have recently come across a collection of anywhere from 2k-5k ceramic molds. From a home I purchased and am in the process of redoing. 

Some molds have been stored in a basement (dark and dank..but not dripping wet)..some were stored in a detached 2 car garage (no heat..but dry)..and several hundred were left outside in the elements.

My question is 3 parts.

1. Will the ones stored in the basement and garage still be viable for sale?

2. Can the ones outside be dried enough as not to be ruined?

3. What is my best option for selling?

90% are strapped..and the other 10% have been stacked flat..with the 2 pieces of each mold meeting to make a whole. Seamlines are visible on the sides. None seem to be warped.

Sorry for such a long post..but any help is appreciated

Link to comment
Share on other sites

I think they mostly will be all fine for use.

The biggest issue with molds is finding a buyer.

Depending on your location  in the country  will determine how easy the sale will be meaning in some areas molds are still used some.

Around here molds are free  as they are to hard to sell.

Link to comment
Share on other sites

you might open some of them to see their interior condition.  the ones outside will probably be very poor quality, nobody in business would put good molds outside to be destroyed by the weather.  they are heavy and were probably put outside just to get them out of working space.

look for crisp edges and details.   if not there, your molds are trash.   to see their quality, push a piece of soft clay into the most detailed area and look at the result.  

 

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.