hi dears
I want to have glaze recipes in 900'C temprature whithaout stain and whit colorant oxides
does any one can help me?
thank you

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,211 posts
  • LocationRed Lodge, Montana

Posted 16 January 2011 - 09:09 AM

Dear Naghmeh,
900 C is cone 010. That is an unusual temperature for glaze firings. After a fast google for glazes , so far I have not found anything below ^08. I know they exist. Try googling. I searched my library and so far, I have not found any clazes for the temperature. Sorry I can't help.
Good luck.
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 Rob Hendriks

Rob Hendriks

    Member

  • Members
  • PipPip
  • 19 posts
  • LocationThe Netherlands

Posted 16 January 2011 - 10:09 AM

I think you need a high amount of a glazefrit with a low melting point, in your glaze recipe.Some lead and glas frits have low melting points.
Rob Hendriks

http://www.reliefs.nl

#4 naghmeh

naghmeh

    Member

  • Members
  • PipPip
  • 26 posts

Posted 17 January 2011 - 09:04 AM

Dear Naghmeh,
900 C is cone 010. That is an unusual temperature for glaze firings. After a fast google for glazes , so far I have not found anything below ^08. I know they exist. Try googling. I searched my library and so far, I have not found any clazes for the temperature. Sorry I can't help.
Good luck.
Marcia



thank you for your reply

#5 naghmeh

naghmeh

    Member

  • Members
  • PipPip
  • 26 posts

Posted 17 January 2011 - 09:06 AM

I think you need a high amount of a glazefrit with a low melting point, in your glaze recipe.Some lead and glas frits have low melting points.