Hey,

I'm not sure what you're trying to do with the black wax.

I went to a Makenzie Smith site and didn't see any "fine lines" related to your needs.

If you're trying to do some kind of fine wax resist lines,

try the tube waxing with liquid wax, or

make a brush with 3 or 4 bristles about 2 inches long and use it the same method as

      incised trailing, dragging it across the vessel, like the Pueblo or San Alfonso do, or

experiment with wax soaked kite string, tack it in place then put the heat from a hair dryer on it.

Good luck.