I was doing my every 4-5 year wash job and I was loading up some bowls with epk for calcining for my wash formula.

Heres how I do it in some green bowls as well as one cracked bisqued one I use just for this purpose .

You can use whatever form you have as it all just comes out and after you blow or towel out the form its ready to glaze.