Hi,

 

I want to recreate old (16th century) tiles from Antwerp (with some protest against the extreme catholic Spanish king Philips II).

In that period, ceramists used a lot of lead glase. It even gave a light yellow impression on the white engobe  they used as an contrast on the red-brown tiles to show the pattern..

 

What can I use as a safe alternatif that ressembles the old glase?

 

Thanks,

Ronny

Ostend

Belgium

Link to comment
Share on other sites

Is  the yellow on the white engobe merely the colour of the white earthenware on firing? If so some of the fritted clear glazes with a good firt for your body would do the trick. 

I say this as I use a white slip over red clay and with a clear it comes out a light cream, definitely not white.

Link to comment
Share on other sites

Thanks for the answer. It seems the light yellow tone comes from the lead glase, so I will have to copy the colour.

 

I will include a link to a pdf-file describing the archaeological finds in Antwerp with many (small) fotos of tiles or parts of tiles. 

 

Which recipy or fritte can you recommend me?

 

https://www.dropbox.com/s/pogy5359jc8c32e/Rapport_7_Inlegtegels.pdf?dl=0

 

Regards,

Ronny

Ostend,

Belgium

Link to comment
Share on other sites

Hey,

 

I think lead glaze is only bad for modern utilitarian vessels such as cups and bowls.

Lead glazed tiles should be ok to make and use as asthetically pleasing replica wall tiles.

 

On the other hand, glaze preparation might be an issue, with dust, stirring and splashing the

glaze around. 

 

good luck,

Alabama

Link to comment
Share on other sites

working at low fire temps you have a lot of options for coloring a glaze. I would first find a glaze that has the qualities of glossiness and movement that you want, then experiment with adding stains and/or opacifiers to get the color you want. It's doubtful that there's a recipe that will work perfectly, so if you're not familiar with glaze formulation then I would look at commercial glazes. If you Google search for low fire glazes you should have no problem finding some to test. The biggest problem will be finding materials in Belgium that can be substituted.

 

If you have access to frits, I would start testing frits plus 10% kaolin for a basic low fire clear.

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.