ashraf elhamy Posted August 30, 2014 Report Share Posted August 30, 2014 Dear All Can any one discuss to me how is the alumina works as stable agent in the glaze ???? Regards Link to comment Share on other sites More sharing options...
ayjay Posted August 30, 2014 Report Share Posted August 30, 2014 Have a look at this below, see if it helps. http://seco.glendale.edu/ceramics/glazecomposition.html Link to comment Share on other sites More sharing options...
Colby Charpentier Posted August 30, 2014 Report Share Posted August 30, 2014 Short answer: High melting point. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted August 30, 2014 Report Share Posted August 30, 2014 Another short answer:the ratio between the Alumina and the silica determine the texture of the glaze. The ratio between the fluxes and the silica determine the melting point. --very brief description Marcia Link to comment Share on other sites More sharing options...
ashraf elhamy Posted September 9, 2014 Author Report Share Posted September 9, 2014 Dear Marcia Could you discuss more detailed information How is the ratio between alumina and silica determine the texture of the glaze Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted September 9, 2014 Report Share Posted September 9, 2014 http://digitalfire.com/4sight/glossary/glossary_silicaalumina_ratio_sio2al2o3.html Link to comment Share on other sites More sharing options...