      Ceramic Arts Network is looking for two new forum moderators for the Clay and Glaze Chemistry and Equipment Use and Repair sections of the Ceramic Arts Network Community Forum. We are looking for somebody who is an active participant (i.e. somebody who participates on a daily basis, or near daily) on the forum. Moderators must be willing to monitor the forum on a daily basis to remove spam, make sure members are adhering to the Forum Terms of Use, and make sure posts are in the appropriate categories. In addition to moderating their primary sections, Moderators must work as a team with other moderators to monitor the areas of the forum that do not have dedicated moderators (Educational Approaches and Resources, Aesthetic Approaches and Philosophy, etc.). Moderators must have a solid understanding of the area of the forum they are going to moderate (i.e. the Clay and Glaze Chemistry moderator must be somebody who mixes, tests, and has a decent understanding of materials). Moderators must be diplomatic communicators, be receptive to others’ ideas, and be able to see things from multiple perspectives. This is a volunteer position that comes with an honorary annual ICAN Gold membership. If you are interested, please send an email outlining your experience and qualifications to jharnetty@ceramics.org.
Sign in to follow this  
Isculpt

What Causes Smoke Patterns In A Foil Saggar?

Recommended Posts

This is probably obvious to everyone but me, but let's say I put a pot into a trashcan with sawdust and wood.  When the sawdust and wood burn, they create smoke which gets on the pot creating color/shadings.  If I wrap the pot in a foil saggar before putting it in the trashcan with the sawdust and wood, how does it get color/shadings?  Doesn't the saggar block the smoke?  I know I'm going to be embarrassed when someone points out something exceedingly obvious in this process that I should already know.....

 

And while we're on the subject, why do people use masking tape to make patterns on a pot that they're going to fire in a trashcan firing instead of using wax to block the smoke and create those patterns?

 

Jayne

Share this post


Link to post
Share on other sites

Foil sag gars that I do are not fired in a smoky trash can. They are fired with the colorants, chemicals, combustibles inside the foil sealed around the pot. II fire them in a raku kiln.

Russel Fouts uses masking tape resist in his foil sag gars with combustibles sealed in foil. Wax burns off way too early to leave a result of resisting smoke.here is his article on smoke firing in an electric kiln.

http://users.skynet.be/russel.fouts/Files/OhYesYouCanPMIJA09lr.pdf

 

Marcia

Mark McCombs likes this

Share this post


Link to post
Share on other sites

What a fantastic article, Marcia!  Instead of the trashcan and all the hassle of building a fire, I'm now planing to use my old kiln that sits on a covered porch.  I was planning to use root kill, copper carbonate and rock salt, but he writes:   "Aluminum foil starts to break up and become flaky between 1200°F (650°C) and1290°F (700°C). This means that most coloring oxides cannot be used because they have little effect below thesetemperatures. In addition, salts can attack the aluminumfoil, breaking it down."  May I ask what your favorite additions are?  So many of the things that are used in traditional western Native American firings are much more readily available in dry climates.  (Dried cow/horse/sheep dung?  Really?  When it rains every darned day here?!)

 

Thank you for sharing the article!  Jayne

Share this post


Link to post
Share on other sites

Read more of his articles. They cover all types of resists down to lipstick. It is different from ceramic sag gars that are fired in a raku kiln and that uses things like copper carbonate and salt. The ceramic saggars for to 1650. The foil saggars in a raku kiln goes 1250-1400 F.It all depends on what your doing. Cow dung is more for a pit firing with pots going over hot coals, then covered with dried dung until it burns through...about 2-3 hours.

 

Marcia

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.