JoLinDesigns Posted August 15, 2014 Report Share Posted August 15, 2014 I am making a rather large, slightly curved bullnose. I will need to glaze one end of it. Since it is large (12 "x10") I fire resting on the shelf. But I'll need to glaze one long end of it. What is the best way to support this so not to glaze it to the kiln shelf? Thanks. Linda Link to comment Share on other sites More sharing options...
JoLinDesigns Posted August 15, 2014 Author Report Share Posted August 15, 2014 Here this shows the actual curve. Thank you. Link to comment Share on other sites More sharing options...
Mark C. Posted August 15, 2014 Report Share Posted August 15, 2014 You could build a clay support that holds it like in your photo from some slabs of clay. It should fire along with the tile so they shrink the same. Mark Link to comment Share on other sites More sharing options...
JoLinDesigns Posted August 16, 2014 Author Report Share Posted August 16, 2014 Thanks. I'll do that. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.