Hi all!

 

Does anyone know how this cross is made? What kind of technique is used? I mean raw form and the glazing/painting part?

 

As far as i know it is supposed to be made of ceramics. Hope the image can be seen properly.

 

Thanks in advance

 

Nandor

Attached Files

  • Attached File  1.JPG   166.18KB   5 downloads


#2 Tyler Miller

Tyler Miller

    Advanced Member

  • Members
  • PipPipPip
  • 592 posts

Posted 04 August 2014 - 11:50 AM

Almost looks more like enamel than ceramic. Does it have a metal backing?  



#3 Lorraine76

Lorraine76

    Member

  • Members
  • PipPip
  • 23 posts

Posted 04 August 2014 - 11:57 AM

i dont think so, i got the information that it is ceramic. But looks very special.

The side looks dark though.



#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 5,813 posts
  • LocationBrownsville, Texas

Posted 04 August 2014 - 01:05 PM

I think it is a pressed image with cuer de seco

which is a resist line with a dark oxide to keep the colors separated.


Marcia Selsor, Professor Emerita,Montana State University-Billings
Marcia Selsor Studio Moving to Red Lodge, Montana Dec 2016
http://www.marciaselsorstudio.com

#5 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 3,044 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 04 August 2014 - 01:33 PM

agree with Marcia.  if you are not familiar with this technique and do live in the USA, you may have seen plastic cookie cutters that have a design built into the interior of the outside shape.  think santa claus with his suit belt, buckle, boots, bag.  when used in cookie dough, the outer shape is cut and the interior lines are formed by pressing into the dough but not cut through.

 

this looks like it was made that way.  then colors added as appropriate.


"putting you down does not raise me up."

#6 Lorraine76

Lorraine76

    Member

  • Members
  • PipPip
  • 23 posts

Posted 04 August 2014 - 02:01 PM

thanks. for the help. Dont live in the USA, but know these kind of cookie cutters.

Could you tell me where i can find more on the glazing/painting technique? - cuer de seco



#7 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 5,813 posts
  • LocationBrownsville, Texas

Posted 04 August 2014 - 05:02 PM

It is actually spelled Cuerda deco "dry line: in Spanish.Here is an explanation from malibu tile

 

http://www.malibutil...Techniques.html


Marcia Selsor, Professor Emerita,Montana State University-Billings
Marcia Selsor Studio Moving to Red Lodge, Montana Dec 2016
http://www.marciaselsorstudio.com

#8 Lorraine76

Lorraine76

    Member

  • Members
  • PipPip
  • 23 posts

Posted 08 August 2014 - 11:37 AM

Hi All!

 

thanks for your useful replies. We found some videos and checked the malibutile site. It is really helpful.

Unfortunately we didnt find anything about the needed materials to be able to try this.

Do you know where we could purchase this kind of material?



#9 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 5,813 posts
  • LocationBrownsville, Texas

Posted 08 August 2014 - 12:30 PM

Atoofsa sells a black wax resist for this purpose. There may be other sources.

 

 

Marcia


Marcia Selsor, Professor Emerita,Montana State University-Billings
Marcia Selsor Studio Moving to Red Lodge, Montana Dec 2016
http://www.marciaselsorstudio.com




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users