i was just glaze firing and a huge storm came then blackout. The kiln was at about 700 celsius when it turned off. Now the blackout is over, but cannot turn the kiln off, because there is still a storm.

I usually fire at 1020 Celsius.

Do you think if i refire the goods tomorrow, they will be ok? No damage happened in there?





Share this post

Link to post
Share on other sites

Looks like you fire to about Cone 05, which is what I do in my classroom.  I had the same problem there, where some spring storms went through and knocked out the power.  


You'll be fine, just firing the kiln as normal, whenever your get around to it.

Share this post

Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  


Important Information

By using this site, you agree to our Terms of Use.