I'm looking for scholarly source of. Why you shouldn't bisque and low fire glazed wares at same time. Or at least some one scholarly saying it. Or the science of why not published somewhere.

 

Thanks in advance

Share this post


Link to post
Share on other sites

I thought the only reason why it wasn't done was the inefficiency of keeping your bisque well-spaced.  I know the old European updraft bottle kilns sometimes had bisque on the top, glaze on the bottom.

 

But I don't know, is there another reason?

Share this post


Link to post
Share on other sites

Off gassing of orgainics(from greenware) can affect some glazes other than exploding greenware thats all I got to say .

I have done low fire but it was in the early 70's and was on another planet.

Mark

Share this post


Link to post
Share on other sites

I bisque and glaze at cone 06 all the time. Bisque in the bottom where elements are cooler. Rather than having two half kiln loads of student work, I put them all together. Marcia is correct. If you have a lot of red or orange glaze, you have to fire separately.

My own work I bisque at cone07, and reduction fire at cone 10 in a gas kiln, so the point is moot.

TJR.

Share this post


Link to post
Share on other sites

I have done a bisque and low fired glaze at the same time with some success. I fire the kiln as I would for a bisque..which is slowly. I also make sure the glazed pieces are on their own shelf in the kiln to minimize any exposure to off gasing. So far I have not had any problems doing it this way.

Share this post


Link to post
Share on other sites

 .I have done low fire but it was in the early 70's and was on another planet.

Mark

Kal-El?

 

I occasionally fire my low fire bisque and glazeware together.  I have actually done it less and less, over the years.  It seems that every time I try, there is a piece being bisqued, that explodes, and sticks to the glazeware.  No matter how much I try and dry the wares, and even putting the bisqueware on the bottom/ glaze on top, it just seems to happen.  It's probably due to the fact, that when I would fire them together, it was because it was then end of the term and I was rushing to get everything done.  

I'll still do it on occasion, if I absolutely have to.

Share this post


Link to post
Share on other sites

This is an excerpt from the above link in reference to the effect of mixed firings in kiln.

"Before the prevalance of encapsulated cadmium stains in red and pink and other such glazes .... the lead based low fire cadmium sulfide (CdS) based reds were susceptible to the sulphur dioxide given off by bisque firing clay. Hence the "admonition"."

best,

........................john

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×