If you are referring to cleaning, as in getting rid of old kiln wash and glaze, this is what I use:

 

https://www.continentalclay.com/detail.php?PID=542&cat_id=193&sub_categoryID=61

 

For the really large drips, they usually just come right off by hand, due to my excellent kiln washing..., and if not, I use a flat heat screw driver to pop them off.

Link to comment
Share on other sites

Would you like eggs and toast with your links?

 

Would not recommend the diamond pads . . . you'll eat through a ton of them. We just cleaned 21 shelves from a salt firing . . . used carbide grinding stones, stiff putty knives, chisel with hand protector; so serious glaze runs so the angle grinder stayed at the workbench. For small glaze drops, a flat-headed screwdriver and hammer work. You just need to learn how to angle the knife/screwdriver/chisel so that you catch under the lip of the glaze bead. For bad glaze runs, grinder.

 

And, in all situations . . . wear your respirator, eye protection, and work gloves (no cheap cloth gloves); slivers of glaze can cause serious cuts. And never run your bare hand over the kiln shelf to see if there are any glaze spots that need removal.

Link to comment
Share on other sites

Guest JBaymore

I use diamond on an angle grinder on silicon carbide and Advancers.

 

When they need a big going over.... take them to the sandblaster and say "me em' black again.  Simple.  No hazard.

 

best,

 

..................john

Link to comment
Share on other sites

I wrote a whole thread with photos on this  subject and covered my tools and grinders  and everyone chined it on thier ways-Just look it up

I did not do any videos sorry

I would like my toast firm and eggs cooked well.

Mark

Link to comment
Share on other sites

Well the group studio I'm at has some, poorly old kiln was shelves

 

For the ones old crusty flaking kiln wash, Is it necessary to grind it all off , to the shelf. Or just smooth?

 

Some shelves are chipped, is there a need to try and fill these chips?

 

Yes mark saw that post. No bacon with breakfast?

 

For,non diamond grinding is this what you all are using?

 

http://t.harborfreight.com/4-inch-diamond-turbo-cup-wheel-98772.html?utm_referrer=https%3A%2F%2Fwww.google.com%2F

 

There is this one shelf out back that has a whole cup,still attached, it looks like it's been there for years. I really want to get that off without killing the shelf.

Link to comment
Share on other sites

I use diamond on an angle grinder on silicon carbide and Advancers.

 

When they need a big going over.... take them to the sandblaster and say "me em' black again.  Simple.  No hazard.

 

best,

 

..................john

Waaaait a minute. I thought advancer and silica carbide didn't gunk up with glaze. Are you grinding from ash firing?

Link to comment
Share on other sites

There is this one shelf out back that has a whole cup,still attached, it looks like it's been there for years. I really want to get that off without killing the shelf.

 

Hahahahaha!....  You should take a picture of that, and post it in the studio with the caption, "Don't Forget to Claim Your Work".

 

I approach applying kiln wash, the same way I approach painting the exterior woodwork on my house; scrap any of the loose bits off, anything that doesn't come off with a thorough scrapping, won't cause any issues.

You don't need to fill in the chips, just coat them, as you do with the rest of the shelves.

Link to comment
Share on other sites

Guest JBaymore

 

I use diamond on an angle grinder on silicon carbide and Advancers.

 

When they need a big going over.... take them to the sandblaster and say "me em' black again. Simple. No hazard.

 

best,

 

..................john

Waaaait a minute. I thought advancer and silica carbide didn't gunk up with glaze. Are you grinding from ash firing?

 

Yes....... I fire a noborigama. Regular silicon carbide does "gunk up".

 

And for the Advancers....... most of the time I just use a putty knife to flick off stuff.....not much stuicks (but for about $250 a shelf... they should even stack themselves). My point was that I am not using diamond on clay ar alumina shelves.... hard to not eat a hole in thiose instantly. But sometimes the kiln wash builds up and gets uneven more than I like. And I DON'T like getting exposed to repeatedly fired stuff that contains microcrystalline silica in the cristobalite form (fired kiln wash)... hence the sandblaster comment.

 

repeatedly fired kiln was dust.... BAD stuff.

 

best,

 

.......................john

Link to comment
Share on other sites

I use two tools

From graiger a silicon grinding CUP it large and does heavy duty work on a 9 or 7 inch milwakee grinder threaded shaft

this is for silicon and dry pressed high alumina shelves

98% of the time I use a makita 4 inch grinder with masonary wheels from harbor frieght sold in 10 packs-I also us a diamond wheel like the one you show but it will eat shelve fast so I am very carfull; with it

This  small 4 inch grinder tool is easy to hold

I have one hanging next to car kiln

My advancer shelves rarely need any grinding

I mostly grins my salt shelves but even those need little as dry pressed high alumina does not attract salt.

Mark

Link to comment
Share on other sites

 

 

best,

 

.......................john

 

 

They don't?!!!

 

I figured it was like something out of Harry Potter; flick your wrist, and the shelves float into the kiln to load, and once done firing, another flick of the wrist and they put themselves away.  Pffff, so much for the "Advance" portion of the name...

Link to comment
Share on other sites

4" diamond cup wheel  (suitable for standard 4.5" hand held grinder)

 

http://www.homedepot.com/p/RIDGID-4-in-Double-Row-Diamond-Cup-Wheel-HD-AWD40/202884364

 

or just the standard 4" diamond cuttoff wheel for the grinder.  This one will leave u shaped divots if you are to aggressive with it

http://www.homedepot.com/p/QEP-4-in-Premium-Diamond-Blade-for-Wet-or-Dry-Cutting-Porcelain-and-Ceramic-Tile-6-4003Q/100140124

 

they also make small 1" versions for your dremel if you need to blend drips off the bottom of your glazed pots/bowls etc.

Link to comment
Share on other sites

I'd love to see that.

Not to mention that some here uses fish in his designs.

And the outdoors are great for creative inspiration

And some fresh salmon would be amazing right now, smoked salmon!, gravlax, salmon sushi, sashimi, ........lucky bears!!!

There is prolly some granite content in rocks, which means there prolly is some feldspar in video also. not to mention silica,

 

It's video source of glaze material.

Link to comment
Share on other sites

  • 2 weeks later...

1st grinding session done!

 

Bought this.

 

http://t.harborfreight.com/4-inch-angle-grinder-91222.html

 

And this

 

http://www.toolocity.com/index.aspx/ImageGallery/Index?productId=2003

 

The old wash and drips big and small came off like butter

 

Less than 2 minutes per shelf,

 

I did eat through 100 grit pad, maybe a bit overkill I may try a different pad next time, or maybe lower grit. And or the stone that came with grinder.

 

It took longer for me to set up and break down than grinding 5 22" shelves

 

It wasn't the chore everyone groans about.

Link to comment
Share on other sites

Guest JBaymore

It wasn't the chore everyone groans about.

 

Try 60-80 shelves at a time between woodfirings.  ;)

 

best,

 

...............john

Link to comment
Share on other sites

Do you grind between every firing?

Do you kiln wash for woodfiring?

 

60-80

(Isn't that why you have students)

I'd invest in a sandblaster

 

Maybe I'll just continue to pay to have my work fired.

 

Nah I still want my own....

Link to comment
Share on other sites

Guest JBaymore

This is for my personal kiln....... no students.

 

Yeah.... generallly at least touch up shelves between every firing.

 

Every so often.... send em' out for blasting.

 

Woodfiring is for masochists. ;)

 

The collge's anagama is bring built in August.  Then the students can learn the fun of "be careful what you wish for". :lol:

 

best,

 

...............john

Link to comment
Share on other sites

This is for my personal kiln....... no students.

 

Yeah.... generallly at least touch up shelves between every firing.

 

Every so often.... send em' out for blasting.

 

Woodfiring is for masochists. ;)

 

The collge's anagama is bring built in August.  Then the students can learn the fun of "be careful what you wish for". :lol:

 

best,

 

...............john

I wouldn't mind partaking in a wood firing sometime.  This is despite the fact, that I've seen your whole right up, on everything that goes into it...

 

By the by, how big is the interior space of the anagama kiln?

Link to comment
Share on other sites

Guest JBaymore

Benzine,

 

It is deliberately a relatively small anagama.  One of the design constraints.  We want to be able to fire frequently within the context of the overall academic program's needs, and with not too large a crew needed for each firing.  It is almost exaclty 200 cubic feet.

 

best,

 

...............john

Link to comment
Share on other sites

Benzine,

 

It is deliberately a relatively small anagama.  One of the design constraints.  We want to be able to fire frequently within the context of the overall academic program's needs, and with not too large a crew needed for each firing.  It is almost exaclty 200 cubic feet.

 

best,

 

...............john

 

I can understand that.  It's one reason my Raku kiln is small and portable, because I take it to school, so I can use it with my students.

 

How tall is the anagama you are about to build?  And I guess I should ask, how big is a "typical" anagama?

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.