Jump to content


Photo

Peep Hole Plug Recipe


  • Please log in to reply
6 replies to this topic

#1 justin1287

justin1287

    Advanced Member

  • Members
  • PipPipPip
  • 63 posts
  • LocationColorado

Posted 20 July 2014 - 06:24 PM

Does anyone know the recipe used for making peep hole plugs?



#2 Babs

Babs

    Advanced Member

  • Members
  • PipPipPip
  • 1,928 posts

Posted 20 July 2014 - 07:38 PM

No I've read one for stilts etc. I'll fossick a bit.

i just threw  one a nd trimmed to fit snug. and I've also , my style, just pushed a bit of clay in at a rushed time and plug had gone awol.



#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 5,486 posts
  • LocationBrownsville, Texas

Posted 20 July 2014 - 08:22 PM

I add some grog, paper pulp, or cellulose insulation into raku clay and stick it in the peep.

Marcia


Marcia Selsor, Professor Emerita,
Montana State University-Billings

Marcia Selsor Studio in Brownsville, Texas.

http://www.marciaselsorstudio.com


#4 Min

Min

    Advanced Member

  • Members
  • PipPipPip
  • 1,178 posts
  • LocationCanada

Posted 20 July 2014 - 08:23 PM

If you have a chunk of insulating brick and a sureform you can make one fairly quickly. Makes a dusty mess, respirator a given.

knowing it exists is not enough, get informed, pass it on

Breast Cancer Awareness  


#5 justin1287

justin1287

    Advanced Member

  • Members
  • PipPipPip
  • 63 posts
  • LocationColorado

Posted 20 July 2014 - 08:42 PM

Thanks, but I am looking for the recipe, not other things that will work.



#6 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,527 posts
  • LocationNorthern Virginia

Posted 20 July 2014 - 08:54 PM

http://community.cer...peep-hole-plug/

#7 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 5,353 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 20 July 2014 - 11:37 PM

I have slip cast them with porcelain slip-worked fine.

Mark


Mark Cortright
www.liscomhillpottery.com