Defective Amaco Wax Resist?

Recommended Posts

I just opened a new jar of Amaco wax resist. I bought it a few months ago and kept indoors.

 

I mixed it well, and its appearance is normal. However, when I brush it on, it creates large particles of (I assume) wax on top of the film. After application, it looks like an old paint that has a lot of dry fragments inside.

 

Again, there are no fragments inside the liquid. They're created under the brush while I'm applying wax resist.

 

Did anybody have the same problem? Is there any way to fix the liquid, or I'll need to buy a new one? Microwaving followed by mixing maybe? Or perhaps adding water?

Share this post


Link to post
Share on other sites

OK, after five calls to Amaco and leaving messages and reminders, I finally got their "technical support". They don't know how their suppliers store their products, therefore, I'd need to order from Amaco directly to make sure the product is fresh and works as advertized. And no, they're not going to replace the defective product.

 

Well, next time I order anything, I'll try to avoid Amaco whenever possible.

Share this post


Link to post
Share on other sites

I think it would still work. If you ran a heat gun over the bits they should melt out. (heat gun on low setting so you don't blow it onto the unwaxed parts)  Running the heat gun over then quickly wiping with a scrap of saran wrap leaves a really slick surface like using hot wax.

 

Not a perfect solution but it would save throwing it out.

Share this post


Link to post
Share on other sites

I've had to think back to my emulsions experience.

To make an emulsion like wax and water combine you need to add a third ingredient; an emulsifier.

Beeswax, water and Borax is a good example.

The percentages are important.

If you have too much wax you get a glutenous glob that seperates out from the water.

If you have too much emulsifier it turns gritty. That sounds like what you have.

As an experiment, maybe you could try adding some shredded beeswax back into the mix and carefully heating it up to see if it might smooth out the emulsion.

I really don't know if it will go back the other way.

 

Chris

Share this post


Link to post
Share on other sites

Thank you guys. Good suggestions.

 

Chris, I'm definitely going to try playing with it. My gut feeling was that the wax settles in globules due to oversaturation. In this case more solvent would help. But since this is an emulsion rather than a simple solution, as you rightfully noted, I may need to approach it differently. Thank you.

Share this post


Link to post
Share on other sites

High bridge

Wax is easy to work with-use a  cut sponge or brush to apply -let dry-then glaze pots.I set the pots on paper after waxing as it leaves a ring on a table. With detail work like cover a glaze say on a fish eye I use a brush but for po bottoms with feet I use a water dampened  cut sponge which

I leave in a low palstic cover tub with the wax in it.

have used many waxes but now only use Laguna clay's Mobilcer A

I thin it with a dab of water to sponge the bowl feet.

Mark

 

 
Mobilcer-A is the industry standard for was resist. Water based petroleum wax emulsion for decorating. Glaze is resisted where wax is applied. This wax resist is an excellent ready-to-use product. It has the result of paraffin wax without the mess or danger of heating. Mobilcer-A is thicker than Axner Premium Wax Resist and comes with instructions on how to thin it to your desired consistency.if ordering for shipment to cold regions during the Winter seasons.

Share this post


Link to post
Share on other sites

I'm having the same problem as MichaelP. Also with Amaco brand wax resist. Never had this problem before with other brands of wax resist. It works but it's much more difficult to deal with than usual.

Share this post


Link to post
Share on other sites

I use a water-based resist from Bailey. Every once in a while if it gritty/clumping I add just a tad bit of water-not much-and zap it in the microwave for a minute or so, then whisk it smooth--no problems at all, covers and seals just like new! 

 

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.