Biglou13 Posted July 20, 2014 Report Share Posted July 20, 2014 I've read, and been told japanese raku and American raku are greatly different process. I've read ome information on the japanese tradition. Lineage. Forms, forming techniques, saggar like kiln...... Can someone please educate further on the differences Link to comment Share on other sites More sharing options...
Benzine Posted July 20, 2014 Report Share Posted July 20, 2014 John will no doubt be able to provide an immense amount of information. From what I recall though, Japanese Rakuware tend to be more neutral (blacks and browns), as opposed to a lot of the bright metallics in the West. The processes are slightly different as well, though I don't recall how. Link to comment Share on other sites More sharing options...
Guest JBaymore Posted July 20, 2014 Report Share Posted July 20, 2014 I teach a course and workshops about this. Here's some "boilerplate" text I have written and given out before in answers to email questions about this. ( the "angle" to some parts is in response to specific questions): "And yes, the Japanese are not as open about sharing 'pottery secrets' as American typically are. I've seen the Raku family process when I've been visiting in Kyoto..... and hence some of my knowledge. Plus I speak enough Japanese to converse a bit, and that fact along with being a potter myself leads a sense of trust to interactions when I am there. Plus introductions from one potter to another helps over there. While impeccably polite, it is a pretty closed society to "outsiders". I am fortunate that I have been accepted into their culture. First off..... American raku and the process in Japan known as Raku are quite different. While generalities are always wrong, there are basically two main versions of Japanese Raku wares....... Aka (red) and Kuro (black). Aka is fired a tad colder than Kuro, due to the glaze maturing difference. Both use a simple lead silicate glaze. The black version uses lead and a ground-up black-ish rock from the Kamo Gawa (Duck River) in Kyoto that is high in both iron and manganese. For Aka only, the raw clay body is covered with a high iron slip that is bisqued onto the piece. For Aka only, there is an intermediate "firing" (a smoking really) where the bowls are placed in a brick box, interspersed with wood charcoal. The charcoal is lit. Where the charcoal is in strong contact with the red slipped wares and little air gets to it... it causes "fire clouding" of the slip...... smoke marks. These carbon deposits will later get sealed under the low melting lead glaze...... creating the variegated color surfaces you see on much Aka Raku wares. They are more dramatic after the intermediary smoking... because the early part of the glaze firing causes some of the smoke effects to re-oxidize. But some usually stays trapped in. Both use the same underlying clay body. It is a coarse, open high-fireclay type body, that in fired consistency greatly resembles SOME American bisqued stonewares when it is fired. The clay is pretty non-plastic, and the traditional forming methods take this fact into account. The most common way is to pinch a THICK general form... and then carve the inside and outside to the desired shape. Some is totally subtractive from a solid block of clay. For Aka, the slip does not go all the way to the kodai (foot ring). There will typically be a place where the glaze overlaps past the slip and goes directly onto a small bit of the raw clay body. But the foot area is always clear of glaze. For Kuro, the glaze is applied all the way under the whole piece...... and right onto the entire foot ring. It is stacked on small wads in the kiln that are later ground off. Almost all real Chawan are typically quite light. Raku ones are quite thin.... weight is an important consideration in a Chawan for actual Chanoyu (Tea Ceremony). Raku Chawan are typically at or under 454 grams...... a pound. They average about 13 cm in diameter and about 9 cm in height. The traditional finish firing (the Raku family tradition) process uses a saggar to contain the bowls set into a small kiln that is charcoal fired, and an apprentice/shokunin (workman) runs a set of dual action bellows to get it really hot. For Aka......... the glaze is caught JUST as the glaze still has a little "fizz" in the melting process...... a tad underfierd. The pieces are pulled from the kiln and air cooled....... no post fire reduction and no water quenching happens. Because the tea is in the bowl for such a short period (minutes)... there is no real concern about lead leaching issues. Plus the bowls are washed very well before a ceremony, and then are ritually washed again during the ceremony....so no thin surface deposits of lead oxide coming out of the glaze will be present at use. Most westerners have never been in a formal tea ceremony. They last a few hours. A lot is involved. Along with garden viewing, a special meal, smoking, and breaks between things, there are different servings of tea. First is what is known as Koicha (Thick Tea). Most westerners have never had this. Most who have, don't usually like it. It is a paste of the powdered Matcha and water that is about like latex paint in consistency. Strong flavor and powerful caffeine kick. If there are multiple Guests, the tea for all of them is prepared in one bowl, and the bowl is passed from person to person after taking their requisite sips. Second is is Usucha (Thin Tea). This is the typical "Tea Ceremony" tea that is experienced by most westerners. It is the same Matcha and watrer... but the proportion of tea to water is much less than Koicha. Strong, but not as strong. There might be multiple servings of Usucha. Tea for a single Guest is prepared in a single bowl and after consuming it, the bowl is given back to the Host. Raku Chawan are usually reserved for serving Koicha, not Usucha. In the core of tradition, a Kuro Chawan is reserved for serving only serious dignitaries and royalty. Far from being considered "disposable", Raku wares are the MOST sought after pieces for Chado (The Way of Tea). The prices for pedigreed Chawan (family name......usage...... etc.) are literally astronomical. There is a "tea saying"......... "Raku first, Hagi second, Karatsu third." That is the 'pecking order' in which Chajin (Tea People) hold respect for the types of wares for Chanoyu. The insulating qualities of the open porous body are a strong positive for Chanoyu. Makes the bowl feel good to hold........ warm, not hot. As is the fact that it is NOT vitreous. Not know to most westerners, sound is also an important part of Chanoyu.... and the sound that a whisk makes in a non-vitrified Chawan is VERY different than the sound produced by a vitreous bowl. Raku is "soft" sound...... stoneware and porcelain are "hard" sound. When a Chajin (tea person) plans a Chanoyu (tea ceremony) there is a concept called toriawase. It is hard to translate..... but it is what a choreographers does to a dance performance, and what a conductor does to a classical concert. Sounds that happens during the ceremony is a part of selecting the timing, the objects and so on in the ceremony. Part of good toriawase. ALL Chawan are treated with great respect.... so they don't get broken often. If you were invited to a real Chakai (Tea Gathering) when you handled the bowl....... you would have taken off all rings and watches and necklaces and such. The bowl would be handled ONLY over the tatami mats on the floor of the Chashitsu (tearoom)..... and you'd hold it literally INCHES from the mats when examining it (part of the ceremony). It will be stored in a cloth bag, then a wooden box, then likely another larger wooden box. Only taken out for use. Treated as more precious than gold. As to 'studying tea bowls'....... this is important....... get to someplace where you can study TEA. The Urasenke School seems to be all over the place. There is WAY more to making teabowls that are actually suitable as Chawan than most western potters realize. A lot of the teabowls you see made by western potters will not pass muster of a real Tea Master for Chanoyu use. Many western potters don't CARE about the traditional use.... but if you do........ you need to understand Tea. In fact, I am giving a lecture presentation at NCECA in Providence next spring that is titled, "What makes a teabowl a Chawan?" where i will address some of the stuff that is not as evident as it might be. If you are going.... stop in and say "hi". There you have it. best, .........................john" Here are some student's work in the Aka Raku intermediary firing process. Here are some student's fired Aka Raku Chawan. Link to comment Share on other sites More sharing options...
Tyler Miller Posted July 20, 2014 Report Share Posted July 20, 2014 I had a little post up, but John's is far more complete and thorough than anything I could ever write. The one thing I can add is that digitalfire has an analysis of kamogawa stone in its raw materials section. It's likely inaccurate and they disclaim it as such, but it's a starting place. Link to comment Share on other sites More sharing options...
prtrpotter Posted January 31, 2016 Report Share Posted January 31, 2016 These are the photos from the conference Kuro Raku 2015 (Czech Republic): https://cz.pinterest.com/figulus/kuro-raku-black-raku-charcoal-kiln/ We used the traditional basalt glazes and charcoal kiln. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.