I do not think its 1 to 1-my guess is its more sodium silicate?Darvan is just a better product

here some formulas for slip from Alfreds off the web

you can compare these to yours

 

Reeves Porcelain Cone 7-10 Grolleg 40 Kona F-4 34 Flint 26 Water Darvan #7 35% 0.35% 
Spleth Porcelain Cone 8-10 Grolleg Velvacast Ball Clay 30 12 8 Custer 18 Flint Pyrax 20 12 Water Darvan #7 40% 0.35% 
Hope this helps
Mark