I want/need/desire/MUST HAVE a nice, clear, ^6 yellow glaze! I don't want a mustard yellow, or a poster board yellow. I want Buttercup yellow, or (pale?) Lemon yellow, something "pretty". I have not been able to find a recipe for such a glaze, so am I seeking the impossible?

 

I have a project in the process, but this color is driving me nuts, and keeping my project on hold.

 

Wait.....maybe I was already nuts.....

 

I would appreciate any help.

Share this post


Link to post
Share on other sites

I just posted a yellow teapot on my gallery with a recipe. It can be intensified by reducing the zircopax and playing with the rutile and vanadium stain. You can probably do without the vanadium because isn't isn't food safe,and increase the rutile. The zircopax made it creamier. Vanadium is considered toxic so do not use on surfaces in contact with food.

Marcia

Share this post


Link to post
Share on other sites

I just posted a yellow teapot on my gallery with a recipe. It can be intensified by reducing the zircopax and playing with the rutile and vanadium stain. You can probably do without the vanadium and increase the rutile. The zircopax made it creamier.

Marcia

 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×