Posted 21 May 2014 - 11:18 AM

Thanks Johanna, your explanation is fantastic, guess the big bucks for an altered printer would be the way to go then if one wanted to have glaze colored decals to use as part of their work. 



#22 justin1287

justin1287

    Advanced Member

  • Members
  • PipPipPip
  • 63 posts
  • LocationColorado

Posted 31 May 2014 - 05:57 AM

I ended up ordering my decals from inplainsightart.com.  They print every Wednesday and ship every Thursday which had me sold due to my very short deadline.  I had to make 23 trophies/plates.  I had never single fired, thrown a plate, or used decals before.  Luckly I only cursed the World a few times.  They came out according to plan!  17 done anyways already with a week to go.

Attached Files



#23 Babs

Babs

    Advanced Member

  • Members
  • PipPipPip
  • 2,031 posts

Posted 01 June 2014 - 12:25 AM

Great result! Onto your next commission..



#24 Diesel Clay

Diesel Clay

    Advanced Member

  • Members
  • PipPipPip
  • 1,049 posts
  • LocationCalgary, Alberta, Canada

Posted 07 June 2014 - 08:20 PM

Justin, those turned out nicely!
Just for any Canadians out there, Mariko Paterson over at Forage Studios in Nova Scotia has a decal printing division. She'll do commercial stuff, as well as turn any of your drawings into china paint decals. She is awesome, and is worth checking out.