Plattypus Posted November 20, 2010 Report Share Posted November 20, 2010 Hello all, I am going to my first wood fire early next month. I have done a soda ash fire and am familiar enough with that process to know that even unglazed areas gain a glaze like patina. My question is, when throwing a lid to sit on a gallery, how much play should be allowed? Are the rims generally unglazed (and therefore resisted) and if so will they gloss over and be usable as ovenware or should rims allow for the additional thickness of the glaze? Link to comment Share on other sites More sharing options...