JohnW Posted April 16, 2014 Report Share Posted April 16, 2014 I've recently adopted an older lockerbie EK with bat pins 11.25" apart. Is there any place still selling non-10" bats? Or do I need to buy undrilled bats and drill them myself?? Thanks!! Link to comment Share on other sites More sharing options...
Babs Posted April 16, 2014 Report Share Posted April 16, 2014 I don't use pins, stick the bats on with a doughnut of clay, seems to work, just need to reform it every so often and level it. Link to comment Share on other sites More sharing options...
Mark C. Posted April 16, 2014 Report Share Posted April 16, 2014 You can still buy un-drilled bats-there are less choices. Or you can drill your wheel head to standard pins and they will all fit Mark Link to comment Share on other sites More sharing options...
timbo_heff Posted April 16, 2014 Report Share Posted April 16, 2014 Drill the head to 10" pin spacing: then you can use any and all of the bats on the market! Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.