pamsheavenlycreations Posted April 15, 2014 Report Share Posted April 15, 2014 I am making clay pendants, and am noticing that glazing them is very pretty however the glaze seems to be chipping off. I am hearing that I do not need to glaze the items that I can stain them??? Can I use an oil base paint to do this? What is recommended or tried. Link to comment Share on other sites More sharing options...
Bob Coyle Posted April 16, 2014 Report Share Posted April 16, 2014 Paint is acceptable, but don't give up on the glazing. Give some better info on what you are trying to do, and I am sure you will get all the help you need on this forum. What cone are you glazing too?. what clay body are you using? can you add a picture? what colors do you want? Link to comment Share on other sites More sharing options...