Hi,

I have been researching this subject and have not found much online about it. I have found some recipes that include goldart but have not found much in the way of particular advantages/disadvantages...and when I called rescoe tech support they did not seem to know anything about the subject.

I would be interested to hear of anyone's experience both in deflocculating and casting with this clay as part of a casting body (I would need to use about 25%).

is sodium silicate enough or does it require darvan 7 or some other material to deflocculate?

 

thanks in advance!

 

Link to comment
Share on other sites

A fellow potter has noticed that some goldart has some organics(coal) in it that causes pitting in some glazes.

I recently posted about pitting in a float blue glaze. I later tracked it down to the clay body having organics that were still out gassing.

My test was to glaze 3 different clay bodied with the same glaze and the offending body did and the other did not pit.

Just my experience

Wyndham

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.