When using 2 glazes did you wait till the first glazed surface was dry poss. overnight, before applying the other glaze? with thin ware you may have had quite a thickness difference if you did not do this, would have added to the problem

Yes, we waited at least one day. But in the end using the same glaze solved the problem. Some of the different glaze pieces survived, but only the ones that were thicker.