Let me preface this by saying that I'm not very knowledgeable about ceramics. My understanding of ceramics stops at about the point where I recognize that clay is different from potting soil. My sister, however, is a ceramics major and is extremely passionate about it. One of the methods she uses for making spheres is to cover the outside of a round object with the clay. Currently, she does this with styrofoam balls, but this is a laborious task that involves cutting the balls down to the right size and shape and can be dangerous if the ball comes off incorrectly and winds up warping the structure. She mentioned that using a balloon for this would be ideal as they're cheap and you can just pop them and pull the latex out when you're done, but balloons tend to roll around so you either have to tape them down, which is difficult and fails half the time, or keep them in a bowl, which puts too much strain on the balloon and causes it to burst.

 

With Christmas coming up, I want to get something that would simplify some of the difficulties she's been having with hand building round shapes, but I had a few questions:

1. I did a little research and found that some people fill balloons with sand or cat litter to give them more rigidity, then drain the particles out to pull the balloon out. Is there any way to inflate the balloon with sand or other cheap particulate matter, or do you have to find a slack mold that's already the size you want to use (some mentioned using tube socks, for example)?

2. It's possible that a higher grade of balloon could hold up under the weight of the clay better. Has anyone tried doing this? Did it work?

3. Does anyone have any other suggestions for an easy and cheap spherical mold?

Share this post


Link to post
Share on other sites

I remember one student when I was in school making two part plaster molds from styrofoam premade balls you buy from a hobby store.  When the plaster was set up he would melt the styrofoam away I believe with acetone.  I don't think he poured slip in it, I think he pressed clay in each half and then joined them together.  May be someone will have a better answer.   Denice

Share this post


Link to post
Share on other sites

Let me preface this by saying that I'm not very knowledgeable about ceramics. My understanding of ceramics stops at about the point where I recognize that clay is different from potting soil. My sister, however, is a ceramics major and is extremely passionate about it. One of the methods she uses for making spheres is to cover the outside of a round object with the clay. Currently, she does this with styrofoam balls, but this is a laborious task that involves cutting the balls down to the right size and shape and can be dangerous if the ball comes off incorrectly and winds up warping the structure. She mentioned that using a balloon for this would be ideal as they're cheap and you can just pop them and pull the latex out when you're done, but balloons tend to roll around so you either have to tape them down, which is difficult and fails half the time, or keep them in a bowl, which puts too much strain on the balloon and causes it to burst.

 

I haven't tried to do this... but I'm keen to make some sphere molds, and thus really keen to hear how things work out for you.

 

Unfortunately, I've had multiple people tell me that balloons will warp. The poured plaster exerts pressure, and the balloon's form will warp both symmetrically and asymmetrically (due to unevenness in the latex). Since the goal in creating a sphere mold is to have the most symmetric form possible, this would be a deal-breaker for me.

 

I've been told that you're far better off using rigid spheres (like bowling or bocci balls) or half spheres. I have yet to accumulate any of these and make the experiment, unfortunately.

 

<Edit>

 

D'oh... just re-read the OP, and realized that you're talking about using balloons as a base for forming clay. Totally different scenario... ignore everything I just said. :wacko:

Share this post


Link to post
Share on other sites

I use balloons all the time ... In fact my newest work as seen in the aesthetics section of this forum is all done around balloons.

Use the heavier duty ones ... You can find bags of these in drug stores or party supply stores. No need to pay big bucks but do not get the thin ones.

The trick is to buy different sizes so you can under inflate them ... there should be a soft neck on them. That way when the clay starts to dry it will simply keep inflating ... If you blow it up all the way the stress has nowhere to go. After a day or two of the clay drying and she feels safe that it can hold its shape, simply prick a very small hole in the soft neck part and the balloon will slowly deflate and release from the sides. Pick out the used balloon and all is well.

You can paddle against it and shape your clay without the balloon exploding. She can lay it in a bowl if she does not want a flat bottom.

They can also be filled with sand then sliced open and emptied ... but I have never bothered with this.

BONUS for you ...you get off cheap this Christmas by buying sis a few bags of balloons! : - )

Share this post


Link to post
Share on other sites

Years ago I did art therapy with kids and one of our projects was to create jack o lanterns with slabs formed around balloons. It was a fun easy project.....we weren't concerned with getting "perfect spheres".

Share this post


Link to post
Share on other sites

No. Just fill with plaster to the desired size and tie a knot.

Chris, if you plan to cast a form from the positive form, then yes, use should use a mold release of some type, WD 40, oil, vaseline, etc.

I have cast many different materials for forms and sprigs. Brushing a light coat of cooking oil of. Mineral oil

On details wooden objects worked without any problems.

 

Marcia

Share this post


Link to post
Share on other sites

You can pour plaster on the balloon. Actually condoms work better because they seem to be a heavier latex.

I use various sized balls for spherical molds. I recently made 8" and14" molds.

 

laughing-dog-smiley-emoticon.gif

 

I haven't bought condoms in like forever!

 

"Why, yes Mr Pharmacist, I want to make molds with them.... Really!"

Cavy Fire Studios likes this

Share this post


Link to post
Share on other sites

YOu Guys imbibing on a little xmas cheer??

Go centre some clay!!

Marcia, now you have your ballooon mold, plaster , how do you use it??That is clay on inside, outside, I have a little wine in me and can't get around getting the clay form off or out of the balloon mold!

Don't laugh ser=ious request for hte brain blocked.

Share this post


Link to post
Share on other sites

 

You can pour plaster on the balloon. Actually condoms work better because they seem to be a heavier latex.

I use various sized balls for spherical molds. I recently made 8" and14" molds.

 

laughing-dog-smiley-emoticon.gif

 

I haven't bought condoms in like forever!

 

"Why, yes Mr Pharmacist, I want to make molds with them.... Really!"

 

 

This is the funny part of our (clay) passion, JustPeachy! Marcia is right though, condoms are stronger and work better. They are not really big though....

 

Happy Holidays my friends, with or without wine inside...

 

Evelyne

Share this post


Link to post
Share on other sites

No. Just fill with plaster to the desired size and tie a knot.

Chris, if you plan to cast a form from the positive form, then yes, use should use a mold release of some type, WD 40, oil, vaseline, etc.

 

Marcia

 

Are you sure? I have always avoided oils because it will transfer to the final mould surface. You do not want any oil on the surface of your final mould if you are going to slip cast because oil will screw up water absorption - ruins your mould.

 

Cover the master mould (plaster) with very thin layer of shellac and then few really thin even layers of soap (dish washing soap is probably fine). After it's dry, use soft toiletpaper to wipe off the excess and you are ready to pour your plaster over your master mould.

Share this post


Link to post
Share on other sites

mart, you are right for slip casting. I don't use most molds that way. I use them as press molds. Vaseline was the release of choice when I first started making molds. I really likeWD 40 although it stinks. Pine oil soap was also taught to me as well.I never noticed any problems from using the above for a mold release

 

Marcia

Share this post


Link to post
Share on other sites

For

Large spherical molds I use balls as the positive mold. I cut heavy cardboard to fit half way around the ball, use a clay wall about 1.5 " around the edge! and pour the upper half? Then remove the cardboard, make keys use a mold release and pour the second half..

 

Marcia

Share this post


Link to post
Share on other sites

 

WD 40 although it stinks.

 

What do you mean it stinks? I use it as an deodorant and aftershave!  WD 40 has saved me marriage 6 times and helped me sell 9 used cars.

 

Beware MArt, my partner says that it attracts dust.. you a potter? better try graphite!

Share this post


Link to post
Share on other sites

as long as we are talking balloons...

once i made some pieces by filling balloons with water, tied them, draped slabs around them, then put the whole combo into a net bag, the kind that onions or old style sausages come in..thin plastic netting. i tied off the netting with some cord and suspended the clay/water balloon/netted forms from a low hanging tree limb (i was working outside)

then i paddled them to smoth the seams and impress the net texture and experimented with tying the forms with cord, cinching them here and there, and let them dry to leather hard. removed the cord, the net bag, pierced the aballoon to pour out the water. i ended up with some pretty cool organic shapes which were salt fired. i believe i used porcelain with fiber content for the clay.

 

i wanted to experiment with a different way of making forms. The idea of working on a suspended form rather than a one  built up from a surface intrigued me. plus it was just kind of fun playing with the balloons on a nice summer day. they did look like odd fruits or ausages curing out there on the tree.

Babs and Marcia Selsor like this

Share this post


Link to post
Share on other sites

 

WD 40 although it stinks.

 

What do you mean it stinks? I use it as an deodorant and aftershave!  WD 40 has saved me marriage 6 times and helped me sell 9 used cars.

it is a petrol chemical and is discouraged for use in the classroom.

Marcia

Share this post


Link to post
Share on other sites

If you are good at throwing on the wheel:

Another option is to throw two halves on bats then join together to make a sphere.

Bats make it easy to handle the two halves. I made perfect 6-12 inch diameter clay balls this way.

 

Das, Australia.

:)

Share this post


Link to post
Share on other sites

No. Just fill with plaster to the desired size and tie a knot.

Chris, if you plan to cast a form from the positive form, then yes, use should use a mold release of some type, WD 40, oil, vaseline, etc.

I have cast many different materials for forms and sprigs. Brushing a light coat of cooking oil of. Mineral oil

On details wooden objects worked without any problems.

 

Marcia

So, you're saying here to fill the balloon with plaster? Once it dried, it would make a balloon-shaped hump mold, which would be cool.

Also, if you're using a condom to create a mold, you shouldn't use WD40 or oil as a release agent.

You should use KY Jelly. :rolleyes:

Sorry, somebody had to say it.

Rae Reich likes this

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×