marybell Posted December 2, 2013 Report Share Posted December 2, 2013 Hello, I am new to ceramics. I fired my first bisque test fire and the kiln shut down too soon. ( My Mistake) Can I re-fire my artwork even though it is cooled down? It went10 hours on low, three hours on 2, two hours on 3, then it turned off because I forgot to re-set the timer.The cone did not even melt at all. The art pieces look great. Do I even need to re-fire? Link to comment Share on other sites More sharing options...
Marcia Selsor Posted December 2, 2013 Report Share Posted December 2, 2013 Just start it up again and set the timer. You can probably speed it up since all the waters gone. Link to comment Share on other sites More sharing options...
Brian Reed Posted December 2, 2013 Report Share Posted December 2, 2013 Yes like Marcia said you can refire. However I would speed up that bisque firing. It should never take 10 hours on low. My entire bisque to cone 06 is like 8 hours max. Link to comment Share on other sites More sharing options...
marybell Posted December 2, 2013 Author Report Share Posted December 2, 2013 Thank you, I will post how they turn out. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.