StaceyB2 Posted November 3, 2013 Report Share Posted November 3, 2013 I am newish to the forum (although was staying away for some time because every time I tried to use the site my computer blocked intrusions) and getting back into clay after about seven years off for raising kids/recovering from advanced Lyme disease. As I am youngish, I was not around when Albany slip was readily available. It fascinated me even before I lived in Albany. Before stopping potting, I experimented coating some items with Albany slip substitute in a wood kiln and got some neat results although now I am limited to an electric kiln. I live in the city of Albany with a nice double-lot of hard to garden clay, which I am assuming is likely similar in profile to Albany slip (I live about a half mile away from the mine). I of course plan on experimenting with it but don't know much other than that it fluxes a lot and has a lot of iron content. I have a lot to learn in general in the glazing aspect of pottery. My impression is that Albany slip is somewhat versatile, so what would you do with it? My husband had the idea of getting clay from different areas around Albany and comparing it as we do have friends on the streets surrounding the old mine. If this topic is boring and not fun, feel free to let it die....my last topic got voted 1 star which I thought was hilarious as I was just trying to make sure I wasn't going to melt my garage floor. Link to comment Share on other sites More sharing options...
PSC Posted November 3, 2013 Report Share Posted November 3, 2013 I've got a gallon of the stuff in my studio. It was a gift for clearing out a shed of retiring potter with some health problems. I haven't played with it yet. Link to comment Share on other sites More sharing options...
Mark C. Posted November 3, 2013 Report Share Posted November 3, 2013 I would keep making my black glaze with it-now I use alberta slip. Albany is great at cone 9 and above in my glazes I still have a few 50# bags of albany left. Mark Link to comment Share on other sites More sharing options...
TJR Posted November 4, 2013 Report Share Posted November 4, 2013 I have a life-time supply of river clay from the Red River which was part of the "flood of the century"in 1997.We shovelled bucket after bucket of Albany slip looking clay from the steps of our parliament buildings. The woman who helped me without complaint I eventually married. She had other fine qualities, but she knew how to handle a shovel. I have at least 5, 5 gallon pails of slip clay. Unfortunately, people don't buy black pots here, or even brown pots. TJR. Link to comment Share on other sites More sharing options...
Biglou13 Posted November 5, 2013 Report Share Posted November 5, 2013 Let us know how tests go. Link to comment Share on other sites More sharing options...
Bob Coyle Posted November 5, 2013 Report Share Posted November 5, 2013 If this topic is boring and not fun, feel free to let it die....my last topic got voted 1 star which I thought was hilarious as I was just trying to make sure I wasn't going to melt my garage floor. What is boring to some is music to others. What a cool concept... digging clay in your own back yard. I hope you can come up with some good stuff. There is a clay bank in an arroyo near me that I have been looking at for years. By golly I think I will join you and go dig some up and test it! Link to comment Share on other sites More sharing options...
Marcia Selsor Posted November 5, 2013 Report Share Posted November 5, 2013 I used a cone 9 glaze 50 albany slip with 50 cherry wood ash. It was a sugary golden matt. Marcia Link to comment Share on other sites More sharing options...
Biglou13 Posted November 5, 2013 Report Share Posted November 5, 2013 Give some to you friends at CAD. (Me) Many ,not always, of the products used in ceramics is found under overburden. Meaning you may have to dig to get to the good stuff. I'd be glad to help test Link to comment Share on other sites More sharing options...
StaceyB2 Posted November 6, 2013 Author Report Share Posted November 6, 2013 I'm sure I will be limited by my kiln--I don't plan on going past cone 6. BigLou, if you send me the $$ I will paypal you a small priority box of it. I can't guarantee the purity--I dug up some that appears to be unadulterated while my kids were playing (that is the tough part, as you know people have been digging in the yard for 90 years) . Sometimes while I am gardening I make little pinch pots and leave them to dry on the fence. It would be cool to see what it would do in a wood kiln just by itself. Actually, I am editing this. I am curious and if you really intend on tinkering with it no $$ needed and I will just send it. PM me your address Link to comment Share on other sites More sharing options...
Bob Coyle Posted November 7, 2013 Report Share Posted November 7, 2013 my "shanty Irish" ancestors owened a home in Walkerville Montana. They dug an out house hole and struck copper ore. Sadly enough they had no mineral rights ... As the lawyer said " sorry you own nothing deeper than the grass roots" Link to comment Share on other sites More sharing options...