I was wondering about making decorative logs to go into a gas fireplace.  What kind of clay could/would stand up to the heat?  Any advantage low fire or hi fire? Could the log be glazed or should it be left unglazed?

 

My old logs were just textured concrete.

 

Thanks!

Ayessa



#2 Conniefi

Conniefi

    Advanced Member

  • Members
  • PipPipPip
  • 34 posts
  • LocationChicago

Posted 18 October 2013 - 10:26 PM

i am using refractory slip for some BBQ's I am making. You could use that it should hold up.



#3 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,050 posts
  • LocationGrayslake, IL

Posted 19 October 2013 - 10:21 AM

A flameware body could work.


Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com


#4 Ayessa

Ayessa

    Newbie

  • Members
  • Pip
  • 2 posts

Posted 19 October 2013 - 07:50 PM

Thanks for the input and ideas. :) The studio I work at is low fire only-will either of these work in a low fire kiln?