Yes. I have done this. Bear in mind that adding these colors to a white slip will lighten them. Test first to make sure the colors are right and that the two formulas interact well before using on a good piece. Underglazes have ingredients in them that keep them wet and spreadable longer so this can cause issues.

Share this post


Link to post
Share on other sites

if you have access to the actual mason stain used in the underglaze, you can make a colored slip.  just make your white slip in dry form and add 10% stain to this before mixing in water, then sieve well.

 

my go-to white slip recipe is equal parts (25% each) Silica, EPK, OM#4, and Custer Feldspar.  Very versatile white slip recipe that can be used from earthenware up to stoneware temps.

 

to make your own underglaze, use equal parts (33% each) Clay, Flux, and Colorant -- usually I'll do either EPK or Ball clay, Gerstley Borate or a frit like 3124/3134, then the colorant (oxides or mason stain).  usually i'll use CMC solution as the water for UG.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.