Posted 14 October 2013 - 08:41 PM

This may be a tall order, but I'd like to find a really tasteful, restrained and understated blue or blue/green midrange glaze recipe. Preferably not too glossy, but I could make that work if it was really exceptional...any suggestions?



#2 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 3,044 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 14 October 2013 - 11:52 PM

varigated slate blue from Mastering cone 6 glazes by hesselberth and roy.  sprayed on it is lovely.  i regret dipping it once.