Jump to content
Sign in to follow this  
StudioEast

Firing Thick And Large Flat Clay

Recommended Posts

I have a project for a flat, 1 inch slab (approx. 30 X 50) I do not know how to set the kiln for bisque.

My first attempt was using 07 cone and slow on my skutt. That actually came out okay.

then I continued to the glaze level and did 5 cone fast. Bad, Bad Bad - the board warped and cracked

on all four sides.

 

Does anyone have a suggestion how to fire this piece?

Share this post


Link to post
Share on other sites

I have a project for a flat, 1 inch slab (approx. 30 X 50) I do not know how to set the kiln for bisque.

My first attempt was using 07 cone and slow on my skutt. That actually came out okay.

then I continued to the glaze level and did 5 cone fast. Bad, Bad Bad - the board warped and cracked

on all four sides.

 

Does anyone have a suggestion how to fire this piece?

 

 

Something like that presents several questions, as there are several problems with it. 1) Is your clay grogged, or are you using fiber to strengthen it, or is it paper clay? 2) How are you shelving the piece to fire, on a single shelf, multiple shelves? 3) Are you grogging the shelf to allow for movement of the clay in heating and cooling? 4) What do you plan for a glaze cycle on the next round? Answering these questions might help you to find your way, or at least to give the good people here a chance to comment.

Share this post


Link to post
Share on other sites

Fire slower. Robert Arneson took days to fire his pieces.

Also, how are you stacking this. I would use 1/4" coils extruder and set the piece on them (bisque them first). That lets moisture escape from the bottom and lets heat circulate.

You don't want something that massive directly on the shelf.

Marcia

Share this post


Link to post
Share on other sites

Firstly, the clay is 02 clay - no grog. When I bisque should I put it on coils also? or is stilts enough? My only problem with this firing is that there is nothing else to put in to the kiln at the same time. When I glaze will I do a low fire glaze instead of high? and do I go up slowly as I will in the bisque firing?

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.