Hello everyone, Im trying to make some ceramic rings but im having problems on how should I do the glazing and the firing of the glaze, since the only unglazed part would be the inside of the ring.

 

greetings from Mexico :)



#2 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 3,041 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 30 September 2013 - 09:27 PM

hello, Mexico, what kind of rings are you making, jewelry for the finger or ear or some other kind of thing?


"putting you down does not raise me up."

#3 muller.vergara

muller.vergara

    Newbie

  • Members
  • Pip
  • 3 posts
  • Locationmexico city

Posted 30 September 2013 - 09:38 PM

hello, Mexico, what kind of rings are you making, jewelry for the finger or ear or some other kind of thing?

Here's an idea of what Im trying to make..mixkorings2.jpg



#4 perkolator

perkolator

    Advanced Member

  • Members
  • PipPipPip
  • 418 posts
  • LocationCalifornia

Posted 08 October 2013 - 06:59 PM

how about using a self-glazing body, like egyptian paste?  just stilt the piece on nichrome bar stilts for minimal interference.