I'm not going to pretend to be an expert, as I've only used a limited amount of products, but from my experience you do not use colored slips/ underglaze over glaze.

 

The results I have seen, cause the underglaze to look "foamy", and generally look terrible. 

 

Of course, if you used a low fire underglaze, it would melt at high fire temperatures, so in that case it might work.

Share this post


Link to post
Share on other sites

I imagine it would depend upon the slip composition.  I have used commercial and home mixed underglazes on fired pieces successfully - the trick is getting the underglaze to stay by coating the piece with dilute Elmer's glue or by warming - and refiring to the original glaze temperature (cone 6 in my case).  If the slip is all or almost all clay I would not expect it to work, but some slips approach being underglazes in their composition, with feldspars and fluxes added.

 

I have recently taken up on-glaze painting (china painting) and find this a much quicker and easier way of recovering from booboos.

Share this post


Link to post
Share on other sites

how was the slip made?  is it simply wet clay with color added or is it a formula with several ingredients?  

 

i know that you cannot do what you want if it is just wet clay with color.  

 

where did you get the slip?  lots more info would help.

Share this post


Link to post
Share on other sites

Slip is clay, and so it must follow the same rules of attachment as any other clay- nothing harder than leather hard. If you trail slip onto glaze fired, bisqued, or bone dry work, it will flake off as it dries. Underglazes are a completely different animal, and are formulated to work on leather hard, bone dry or bisque. They may very well work on glazed pots, too.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.